Hello members,
This is from a batch of ceramic cpu's. In total, so far I recovered a 5.7g of TWICE- REFINED gold button. This thing is so shiny, it doesn't need a flash to take a picture, although I did. This button was melted within 15 - 20 minutes after the melting dish was seasoned.
The odd shape is because I thought it was hard enough to lift out, and when I tried to lift it out of the melting dish, it smashed in from the tweezers. The pipe had already started forming before I touched it, but I didn't mind that the button isn't 100% circular.... but it still shines like gold, for sure.
My yields came from 304 ceramic cpu's. There were 145 for one type, and 154 for the other cpu's.. Mixture of AMD's and Athlon's. Until I know for sure there isn't gold in the ceramics, I'm holding on to them. But, as it is, my yields from the cpu's (probably just/mostly pins) are:
Started with: 304 ceramic cpu's. (AMD's + Athlon's).
Recovered 5.7g of .99.9% twice refined gold.
Photos are from my desktop scanner. I have pictures on my phone, but it's been giving me problems and I have to plan when I want to upload pictures from my phone.
Kevin.
[UPDATE] The flux on the bottom is so light, that it plucks off with my thumb nail. The melting dish was never used before the melt.
This is from a batch of ceramic cpu's. In total, so far I recovered a 5.7g of TWICE- REFINED gold button. This thing is so shiny, it doesn't need a flash to take a picture, although I did. This button was melted within 15 - 20 minutes after the melting dish was seasoned.
The odd shape is because I thought it was hard enough to lift out, and when I tried to lift it out of the melting dish, it smashed in from the tweezers. The pipe had already started forming before I touched it, but I didn't mind that the button isn't 100% circular.... but it still shines like gold, for sure.
My yields came from 304 ceramic cpu's. There were 145 for one type, and 154 for the other cpu's.. Mixture of AMD's and Athlon's. Until I know for sure there isn't gold in the ceramics, I'm holding on to them. But, as it is, my yields from the cpu's (probably just/mostly pins) are:
Started with: 304 ceramic cpu's. (AMD's + Athlon's).
Recovered 5.7g of .99.9% twice refined gold.
Photos are from my desktop scanner. I have pictures on my phone, but it's been giving me problems and I have to plan when I want to upload pictures from my phone.
Kevin.
[UPDATE] The flux on the bottom is so light, that it plucks off with my thumb nail. The melting dish was never used before the melt.