kurtak
Well-known member
One more question --- can you provide some pictures of the chips you are wanting to process ?
Kurt
Kurt
kurtak said:One more question --- can you provide some pictures of the chips you are wanting to process ?
Kurt
i am far from my work area today,kurtak said:ashir
Sorry I have not posted more lately - I have been gone on a trip & just got back & as well I am currently sick
Could you provide a better picture of the chips --- I would like to see "more" of what is in the mix of the chips
A few chips in your hand (with the rest in the back ground) does not really tell me much
Kurt
ashir said:thanjs kj!
hope i can do this,
ashir said:kj i read more on what you mention! loosing gold is the mainissue! i am still too afraid of loosing values as gold wires sometimes broken so fine! i still want use smelting mathods as i am also finding ores to be processed! big batches of e waste !
chamicals and labour is still too cheap here. 3 to 7 dollars per 10 hours is labour cast here!
though its hard to find chamicals but these are all cheaps ( out of flourspar) ! the mathod you mention is quite intresting and safe as low waste production!
but i have to run 2 different setups for ewaste and ores! so i was intrested in one in all( hope you understand what i want to say because my english ability is not so good)
but in smelting i am not feeling good to use lead( as it will raise same issue of too much toxic waste)
so i was looking to use silver as collector, copper is a choice if shark start a thread of coper cell( he once ask that soon he is going to do so)
ashir said:thanks kj.
i am working on rotary furnance. crucibles are ready so i am finding some stuff to fix crucibles in rotary furnance setup, i ask gaurave to start a thread on making of rotary furnance at home and a coal fired furnance( if he have time for us)
i want see gaurave because he is in me neighbour country and i can easily get what he will use!
also searching a fume controle idea that i can construct by myself to controle smelting fumes.
i already arranged flux
borax
soda ash
flourspar
kno3 ( its banned, no idea yet to use it but i buy it because may be next time i can not buy )
silica is not yet in my flux but i will get this soon.
what should be the ration of silver to ash
or silver ratio to axpected values?
ashir said:thanks kj. yes rotarg furnance is difficult to prepare at home, but once i will try. and after smeltinv with silver, there is no need of any cupelation! or 2 step smelting is required?
ashir said:thanks kj
i need some more clearification please.
what will the way to skimm off lead while melting the ashes? a rod with bended end will work? or i have to melt , then turn iff furnance remove sold lead with base metal and an other melt with silver?
thanks again for guide