all 1/10th 12k gold filled and marked as such all pieces were all batches are ultra sonic clean, stones and other ferrous metals removed when practical. 1 of the pocket watch chains is 1/10 10k otherwise 1/10 12k. Remember most glasses have a ferrous base metal some guys run reverse AR recovery but there doesn't seem to be much stainless we always run 50/50 nitric as normal and never have problems besides the few small stainless pieces that need removed before filtering. If you are one of the paypal only kinda people you have to purchase of ebay and we charge 13% more to cover fees.
Avg recovery for us on the these same NOS glasses is 3.8% to 4.1% with our best being 4.3% worst was 3.11%w offer a 3% discount on ach or wire transfers google, apple, and bitcoin if you are in Kansas City 5% discount on cash 3% on checks. PM if interested guaranteed recovery of 3% as long as your accountability rate is in the mid 90s we average 3.8% on the old frames $1.00 per gram with free shipping in the us we will consider offers if it you want to purchases multiple lots.
Avg recovery for us on the these same NOS glasses is 3.8% to 4.1% with our best being 4.3% worst was 3.11%w offer a 3% discount on ach or wire transfers google, apple, and bitcoin if you are in Kansas City 5% discount on cash 3% on checks. PM if interested guaranteed recovery of 3% as long as your accountability rate is in the mid 90s we average 3.8% on the old frames $1.00 per gram with free shipping in the us we will consider offers if it you want to purchases multiple lots.