Processed about 215 cm2 CPU caps with gold on both sides, so, gold plating surface area was approx. 430 cm2. The caps weighted about 70 gr, there was some solder remained on each cap. Got about 3 gr of gold.
Lets calculate the thickness out of this figures. The volume of gold is 3 gr : 19,3 g/cm3 = 0,155 cm3. The thickness of gold layer is 0,155 cm3 : 430 cm2 = 0,00036 cm = 3,6 um. What do you think, is it real?
Lets calculate the thickness out of this figures. The volume of gold is 3 gr : 19,3 g/cm3 = 0,155 cm3. The thickness of gold layer is 0,155 cm3 : 430 cm2 = 0,00036 cm = 3,6 um. What do you think, is it real?