The melting point of Gold, Silver, copper and other metal below 1400℃ can be melted by graphite crucible.
Melting point over 1400℃ should be melted by quartz crucible. (quartz crucible is heating by metal induction)
The melting point of metal powder over 1400℃ is not suggested to use this melting furnace.
Melting the metal powder by quartz crucible, the amount of metal powder must be up to 70%.
Specification:
Max Melting Capacity
1KG (Gold/Platinum)
2KG (Gold/Platinum)
Voltage
220V; 50/60Hz; Single phase
Power
5000W
Meltable metals
platinum, palladium, stainless steel, gold, silver, copper and other alloys
Melting time
2-3 minutes
2-5 minutes
Max temperature
2100℃
Cooling system
water cooling (circulating water, pump water)
Dimension
620*360*380mm
Weight
32kg
Stainless steel jet self-priming water pump Param eters:
Voltage: 220V/50Hz
Power: 0.37KW
Current: 2.4A
Rotation speed: 2900r/min
Pipe diameter: 25mm
Rated flow rate: 1.5m³/h
Max flow rate: 3.0m³/h
Rated lift: 20m
Max lift: 30m
Max suction lift: 8.5m
Weight: 6kg
Size: 360*160*190mm
$1000 shipped
Melting point over 1400℃ should be melted by quartz crucible. (quartz crucible is heating by metal induction)
The melting point of metal powder over 1400℃ is not suggested to use this melting furnace.
Melting the metal powder by quartz crucible, the amount of metal powder must be up to 70%.
Specification:
Max Melting Capacity
1KG (Gold/Platinum)
2KG (Gold/Platinum)
Voltage
220V; 50/60Hz; Single phase
Power
5000W
Meltable metals
platinum, palladium, stainless steel, gold, silver, copper and other alloys
Melting time
2-3 minutes
2-5 minutes
Max temperature
2100℃
Cooling system
water cooling (circulating water, pump water)
Dimension
620*360*380mm
Weight
32kg
Stainless steel jet self-priming water pump Param eters:
Voltage: 220V/50Hz
Power: 0.37KW
Current: 2.4A
Rotation speed: 2900r/min
Pipe diameter: 25mm
Rated flow rate: 1.5m³/h
Max flow rate: 3.0m³/h
Rated lift: 20m
Max lift: 30m
Max suction lift: 8.5m
Weight: 6kg
Size: 360*160*190mm
$1000 shipped