Guess what,
I have found an old computer with official gold content of 44 gramms. :lol:
http://ru.wikipedia.org/wiki/ЕС_ПЭВМ
I think it is a full bs.
Has anyone true info of the gold content in those PC.
They are soviet and IBM PC compatible.