I have a little button I finished on Tuesday, 16th 2021. It came from 524g watch bands tops. Well, the tops came out to 524g, but I had 18lbs of them and I think I did about close to half the weight. I will have to refine it again, but it still looks good.
I melted about 9.9g gold this week from material I had. I still have much more to process.
This should hopefully give newbies and professionals at refining more of a reason to do what you do. It's worth it if you're not mainly focused on the MONEY it can bring. I am focused on being able to bring gold to a pure and solid state from scrap. The money will come to you, but focus on learning on refining, and then the money MIGHT come chasing you.
In short, this is a GIFT to know how to refine. In some places, it's not even a privilege to refine LEGALLY, because the acids themselves are BANNED.
I'm so glad to have the opportunity to be a part of a community that is not of the average, in so many aspects.
"Thank you to all of you here on this forum for all of the time and knowledge you have passed along. Believe me, it's being harvested."
scrapparts
I have a little button I finished on Tuesday, 16th 2021. It came from 524g watch bands tops. Well, the tops came out to 524g, but I had 18lbs of them and I think I did about close to half the weight. I will have to refine it again, but it still looks good.
I melted about 9.9g gold this week from material I had. I still have much more to process.
This should hopefully give newbies and professionals at refining more of a reason to do what you do. It's worth it if you're not mainly focused on the MONEY it can bring. I am focused on being able to bring gold to a pure and solid state from scrap. The money will come to you, but focus on learning on refining, and then the money MIGHT come chasing you.
In short, this is a GIFT to know how to refine. In some places, it's not even a privilege to refine LEGALLY, because the acids themselves are BANNED.
I'm so glad to have the opportunity to be a part of a community that is not of the average, in so many aspects.
"Thank you to all of you here on this forum for all of the time and knowledge you have passed along. Believe me, it's being harvested."
scrapparts