the most interesting part i saw t'ill now was under "Connectors, Interconnects "
basically... we get a confirmed source of info about plating thickness....
which is 30 µin (micro inches) or 0.76 µm (micro centimeter) for most kinds of pins....
And a question for GSP or any other expert:
how much does 1 square inch , 1 µin thick of pure gold weight ??
i'm wondering, about your speadheet that you make the calculation of gold plating, what does, dividing the gold spot by 100K give us?
is this the value of 1 sq in , 1 µin thick of gold?
if so... how does it happend?
i know experience taught you that, but i'm feeling somthing is missing in that formula....
Many thanks for your answers
SMAUL
the most interesting part i saw t'ill now was under "Connectors, Interconnects "
basically... we get a confirmed source of info about plating thickness....
which is 30 µin (micro inches) or 0.76 µm (micro centimeter) for most kinds of pins....
And a question for GSP or any other expert:
how much does 1 square inch , 1 µin thick of pure gold weight ??
i'm wondering, about your speadheet that you make the calculation of gold plating, what does, dividing the gold spot by 100K give us?
is this the value of 1 sq in , 1 µin thick of gold?
if so... how does it happend?
i know experience taught you that, but i'm feeling somthing is missing in that formula....
Many thanks for your answers
SMAUL