I am leaching 1 AT of ore with a 1/2 clorox 1/2 vinegar solution. I have been using activated charcoal to capture the gold. So far the results have been from .5 to 2.5 grams per ton AU. I was wondering if removing the magnetics before doing the leach would help? Also would soaking the ore sample in Hydrogen Peroxide before leaching help? Would these two things or anything else help increase my gold level?.