zamistro said:Would any of the acid processes work on this?
Brandt said:have about 3 lbs of black sand from alaska with fine gold in cant pan it out. best way to process?? Have any ideas. Thanks
61 silverman said:Rick; You seem to be very knowing of mercury... Let me give you a brief story of the mercury I have... From the time I can remember my Dad told my brother, sisters and myself too keep our hands off these little jars!! He told us that they are "FULL of GOLD" what they are is two small bottles 2lb-13oz's - bottles included- of MERCURY..by the size of the bottles I guess there is about 2 1/2 fluid oz,
My Question first is HOW MUCH GOLD can be held in say 1 fluid oz. of Mercury. My plan of recovery of the gold is to get a AIR-TORT , and then treat chemically to refine..
also I don't know how old this mercury is !!! I know it is older than 48 years, I think my father had panned the gold when he was a young man with his father..He had it before he married my mother,
I will get a couple pictures up in a couple days.. Thanks Mark
Your question is not clear to me, Mark. Can you please be a bit more specific?61 silverman said:One more question about dental material, When deciding which material has the potential of having mercury,( so needing to be retorted") would that only be items that have material packed into them like an adhesion material? or all parts.!!????