Dear Sir,
I have an electroplating business in India and i use 24 ct Gold for plating.
I used to make my own Gold Potassium Cynaide (GPC) using Aqua Regia method.
My question is, is there any better option for nuetralising Aqua regia solution by Ammonia Solution (Aq) ???
Mustafa.
Surat ( Gujarat )
India.
I have an electroplating business in India and i use 24 ct Gold for plating.
I used to make my own Gold Potassium Cynaide (GPC) using Aqua Regia method.
My question is, is there any better option for nuetralising Aqua regia solution by Ammonia Solution (Aq) ???
Mustafa.
Surat ( Gujarat )
India.