E Elfs Member Joined Sep 18, 2010 Messages 20 Dec 29, 2010 #1 I have 95% Tin 5% Antimony Lead free solder. Will this work for Stannous Chloride? And with Ap. Can the solution just be diluted with tap water and have air bubbled through it to use as Copper etch for fresh pins and finger?
I have 95% Tin 5% Antimony Lead free solder. Will this work for Stannous Chloride? And with Ap. Can the solution just be diluted with tap water and have air bubbled through it to use as Copper etch for fresh pins and finger?
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida Dec 29, 2010 #2 1. Yes. 2. No, you need free oxygen that is not bound like it is in water. Steve
E Elfs Member Joined Sep 18, 2010 Messages 20 Dec 29, 2010 #3 Thanks Steve. Reading the Cupric Chloride doc from your site, clears thing up. And the Antimony will not dissolve easy in acids.