Melt Dishes and Crucible Sweating Mysterious Liquid when heated.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Geber

Member
Joined
Nov 13, 2024
Messages
7
Location
Connecticut
Has anyone observed liquid sweating out of their melt dishes? I have been having this problem and it makes pouring the metal impossible.

Not too long ago I bought some melt dishes, heated one to drive away moisture, glazed it, and melted some fine silver in it with no problems.

Then I used it about a week later and a liquid started coming out of the ceramic when the silver was nearing its melting point. This liquid took a glass-like appearance when cooled, and exploded with a pop when it was quenched. I reasoned it was excess borax, that the dishes somehow came glazed with borax, and that I should not glaze the next one. I then used an unglazed one, and the metal did not stick inside, but the same liquid appeared. It also seems to be taking too long to melt the silver with MAP gas and that I have to use way too much gas.

Finally, I used my graphite crucible in my little furnace. The crucible had also been sitting around in my shop, which can get damp, and I did not condition it. When it got to temperature, I looked in the crucible and saw an orange liquid. It was slightly steaming, convecting vigorously, and spitting out the occasional tiny orange spark. Thinking it was the silver, I poured it into my mold, and poured a bar which was dark-red and blackish in color. I emptied the mold and the "bar" fragmented into pieces. The silver was adhering to the side of the crucible, and was never totally melted. I did not put anything in this crucible besides silver and a little pinch of borax.

Can anyone tell me what I'm doing wrong? Do I have to drive the moisture out of melt dishes and crucibles every time I use them, and is this liquid a saturated water-borax mixture? Thanks!
 
The problem is NOT with the crucibles &/or melting dish's

The problem IS that you are NOT getting all the chem washed out of your precipitated metals &/or that you are having base metal oxides, hydroxides etc. (metal salts not washed out) co-depositing with your precipitated PMs

Kurt
 
The problem is NOT with the crucibles &/or melting dish's

The problem IS that you are NOT getting all the chem washed out of your precipitated metals &/or that you are having base metal oxides, hydroxides etc. (metal salts not washed out) co-depositing with your precipitated PMs

Kurt
Thank you. I will do a better job at washing them next time. How necessary is it to heat a melt dish to drive away moisture after the first time? Do they reabsorb moisture?
 
Thank you. I will do a better job at washing them next time. How necessary is it to heat a melt dish to drive away moisture after the first time? Do they reabsorb moisture?
A properly sealed melt dish, will not absorb moisture on the up ( parabolic) side. The bottom could, depending on clay type used in its manufacture. So could go either way. You did not state the composition of the melt dish, and there are a variety of recipes.
 