Slochteren Well-known member Joined Apr 3, 2015 Messages 175 Location Netherlands Jul 31, 2015 #1 Any PM in this or just garbage?
S shmandi Well-known member Joined Oct 3, 2012 Messages 170 Location Slovenija Jul 31, 2015 #2 According to some information I found Silver-Palladium (Auropal) or Gold-Palladium (Midor) alloys are used for those.
According to some information I found Silver-Palladium (Auropal) or Gold-Palladium (Midor) alloys are used for those.
N nickvc Moderator Staff member Moderator Joined Sep 14, 2009 Messages 5,658 Location birmingham Jul 31, 2015 #3 You will have to test them all of them as there are many white base metal tooth alloys and a few precious metal ones :roll:
You will have to test them all of them as there are many white base metal tooth alloys and a few precious metal ones :roll:
Slochteren Well-known member Joined Apr 3, 2015 Messages 175 Location Netherlands Jul 31, 2015 #4 Thx, also buying just from Picture is a bad idea...
S ssabovic Active member Joined Nov 25, 2010 Messages 40 Jul 31, 2015 #5 it could be paladium alloys, nickel alloys. cobalt alloys....... , or combination of this, you should test each peace . regards
it could be paladium alloys, nickel alloys. cobalt alloys....... , or combination of this, you should test each peace . regards
M meatheadmerlin Well-known member Joined Mar 6, 2013 Messages 108 Location New York Sep 6, 2015 #6 Depending on the age of the pieces, you should also safeguard against the possibility of mercury being present.
Depending on the age of the pieces, you should also safeguard against the possibility of mercury being present.