Anyone know about these chips?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

bhilton

Well-known member
Joined
Jan 17, 2024
Messages
74
Location
London, Ontario
This chip appears to have nice gold but the gold bits in the attached pictures are magnetic. Is it still possible to be gold plated over a magnetic metal?

Sorry i broke it in half and extracted the gold looking bits from the other half already. They stick to my magnet with nothing else attached to them.

Thank you!
 

Attachments

  • IMG_1726.jpeg
    IMG_1726.jpeg
    1.2 MB · Views: 0
  • IMG_1725.jpeg
    IMG_1725.jpeg
    1.3 MB · Views: 0
  • IMG_1724.jpeg
    IMG_1724.jpeg
    1.6 MB · Views: 0
Kovar. An iron based pin that is used in many electronic items. Especially where heat is a factor. Example: pins from many CPU’s.
 