I started with a 10g bar .999,9 pure and trying to dissolve it in AP. Using muriatic acid and 12% peroxide. Have it heated to 155. Been adding peroxide in 15 ml bumps. I’m almost 4 hours in yet the bar still looks in tact.
Is AP bot as good for bullion compared to Aqua Regia. Should I raise or lower temp? Im considering sodium metabisuphite to precipitate out what I do have then starting over with aqua regia.
Any advice would be appreciated!
On a side note I did search for ap temp but didn’t find anything concrete.
Is AP bot as good for bullion compared to Aqua Regia. Should I raise or lower temp? Im considering sodium metabisuphite to precipitate out what I do have then starting over with aqua regia.
Any advice would be appreciated!
On a side note I did search for ap temp but didn’t find anything concrete.