I'm putting together some figures and I want to see if my data is comparable with what everyone processing cats finds.

What do you find to be an average weight for the converter innards?
 
I just reweighed them, individually this time.

One was from a Land Rover and weighed 1.1kg on it's own.
The other 4 came from medium sized cars and weighed approx 0.7kg each
 