T3sl4 said:I've recieved a request for one, so I soon may have more than the prototype to show off. 8) 8)
T3sl4 said:My prototype is built around my welder's 240V, 50A circuit, which is good for 10kW, give or take.
I personally wouldn't recommend induction for aluminum. It's so much easier (and cheaper) to melt with, say, a campfire!
Tim
Lou said:Why so slow for aluminum?
Besides, one can easily construct a propane or oil-fired furnace that'll do a #20 crucible full of aluminum (or more) for under $500. I've done it.
If you plan on doing quality castings in aluminum and want good surface finish, invest in Petro Bond. I don't have any photos to show on my new computer, but the finish was unparalleled. Furthermore, magnesium castings are readily done with it. Check out backyardmetalcasting.com for more details.