ten years ago i made with degussa an assay to know how much gold and silver were present in a kilo of those small rectangular black chips---since then these chips became flat (thinner) and i would like to know if they still contain gold and silver?
the result of the assay ten years ago was:gold=1,o2grams per kilo
silver:11grams per kilo

please if anyone knows something about it,give me a reply---
 
Arthur,

I don't have any exact numbers on the chips (there are just too many types out there), but generally speaking your numbers are not far off ( but a little high) from what I've seen in small samples of modern flatpacks.

Steve
 