- Joined
- Jun 22, 2023
- Messages
- 110
Currently have 5.065 OZ of pure medical grade platinum wire with more on the way. Looks like steel wool! has already been nitric bathed to remove any impurities and will hot water rinse and HCL rinse again before shipping. Guaranteed to be over weight. Will post a picture in a day or 2. Original Platinum base with membrane and silver coating material removed. May contain trace silver, but I don't think it does.
Willing to separate in 1 oz lots. Buyer pays shipping, insurance is optional. Zelle or Paypal when it ships.
edited since I'm an idiot ;-) $650/troy oz ($888 spot price)
Pictures on request and I'll try and post a few in the next day or 2.
PM me if interested. happy to document any experiments within reason to prove purity or arrange sending a sample.
US domestic shipping only. Flat rate USPS.
Willing to separate in 1 oz lots. Buyer pays shipping, insurance is optional. Zelle or Paypal when it ships.
edited since I'm an idiot ;-) $650/troy oz ($888 spot price)
Pictures on request and I'll try and post a few in the next day or 2.
PM me if interested. happy to document any experiments within reason to prove purity or arrange sending a sample.
US domestic shipping only. Flat rate USPS.
Last edited: