Benjaminza
Active member
Can you guys plz tell me if it is possible to depopulate small boards especially with LEDs, resistors and mlcc's on with ap solution.
Yes, but that will also take the Copper.Can you guys plz tell me if it is possible to depopulate small boards especially with LEDs, resistors and mlcc's on with ap solution.
No ordinary full strength.Can you recover the copper later on? Do you mean as in a dilute HCI solution? Is it not a good thing if the copper is put into solution so early in your chemical proses?
Fastest at least, and most of the time most practical.So best way to depopulate is either mechanically or heated?
A compressor is always nice to have, but why do you need one in this discussion?Ok so I then need a compressor too.
I have a air bubbler. I meant a compressor for pumping air into the bottom of my crucible while incinerating my chips to avoid carbon.A compressor is always nice to have, but why do you need one in this discussion?
For bubbling air it is enough with an aquarium air pump, cheap and effective.
I've been recovering and refining for about 6 years now. I can promise you that a decent percentage of the videos on you tube are either misleading, or steps are left out, or are not logical, as far as some are completely bs. Read hokes book, I'm sure you can find it on this forum with ease.Yes I am only starting now. I think I watched almost every video on youtube at least 5 times. Dud recovery in my mind probably 3 more times but to be honest was still soooo overwhelmed with my first attempts.
First time I got a positive stannous test I wanted to cry lol.
I do though have a fume hood and foundry furnace. I have been prepping for a few months.
I do appreciate any and all advice. Ill definitely be watching this post for any other tips.
Thanks guys
I hear you there..seems a lit are just click baitI've been recovering and refining for about 6 years now. I can promise you that a decent percentage of the videos on you tube are either misleading, or steps are left out, or are not logical, as far as some are completely bs. Read hokes book, I'm sure you can find it on this forum with ease.
Enter your email address to join: