i have download the file that shows step by step process of refining? shall i use urea and smb in one time? anyone can help?
 
not same time, Urea is to rid the nitric from Aqua regia, add small amounts till no more fizz,when warmed and PH>1, then dilut solution with water 3 to 4 times, let sit overnight. decant ,filter liquid then use SMB.
boiling off nitric works well very also, if you can not get urea.
 