sena Well-known member Joined Jul 21, 2011 Messages 208 Jun 2, 2012 #1 Good day, could these yield any PM ,the monolithic capacitors. Thanks Sena Attachments IMG_1631.JPG 2.8 MB IMG_1633.jpg 3.6 MB
goldenchild Well-known member Joined Aug 14, 2009 Messages 1,810 Jun 2, 2012 #2 In the second picture the brownish ones are what you are looking for. I believe everything else will be aluminum or some other non precious metal.
In the second picture the brownish ones are what you are looking for. I believe everything else will be aluminum or some other non precious metal.
etack Well-known member Joined Nov 8, 2008 Messages 1,404 Location Dayton, Ohio Jun 2, 2012 #3 the first pic is of chip resistors this is a good thread http://goldrefiningforum.com/phpBB3/viewtopic.php?f=61&t=10215&hilit=chip+resistors Eric
the first pic is of chip resistors this is a good thread http://goldrefiningforum.com/phpBB3/viewtopic.php?f=61&t=10215&hilit=chip+resistors Eric
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida Jun 2, 2012 #4 Yields for monolithics range from zero to 2.5% by weight. Here's some of the earlier posts on the subject: Monolithic Yields Steve
Yields for monolithics range from zero to 2.5% by weight. Here's some of the earlier posts on the subject: Monolithic Yields Steve