Well-known member
Dave - this is another thread where links I posted are not working
Those links are VERY important - without them the info I posted is incomplete
Especially the links to stannous testing that show (pics) of "false" positives that you can get which can cause someone to believe they have PMs in solution when in fact they don't which in turn cause people to waste time & become very frustrated trying to recover PMs that just are not there
Can you please fix my links in this thread
Kurt
Those links are VERY important - without them the info I posted is incomplete
Especially the links to stannous testing that show (pics) of "false" positives that you can get which can cause someone to believe they have PMs in solution when in fact they don't which in turn cause people to waste time & become very frustrated trying to recover PMs that just are not there
Can you please fix my links in this thread
Kurt