Geo Well-known member Joined Mar 1, 2011 Messages 7,070 Location Decatur,Ala. Jul 20, 2018 #1 Cemented silver from various sources. Assayed at 99.6% silver. Attachments 100_1883.JPG 267.5 KB · Views: 265 100_1884.JPG 278.5 KB · Views: 265
MGH Well-known member Joined Sep 28, 2012 Messages 252 Location Nebraska, USA Jul 20, 2018 #2 I'm calling you out, Geo. That little bar on the right is too yellow. There's no way that's 99.6% silver. It's still a nice part of the collection though
I'm calling you out, Geo. That little bar on the right is too yellow. There's no way that's 99.6% silver. It's still a nice part of the collection though
Geo Well-known member Joined Mar 1, 2011 Messages 7,070 Location Decatur,Ala. Jul 20, 2018 #3 Yea, the little one was a little contaminated. 99.1% gold and .9% silver. It was really bad. :-D
F fishaholic5 Well-known member Supporting Member Joined Jun 5, 2018 Messages 183 Location Australia Aug 3, 2018 #4 They look good 8) I hope my efforts at pouring Silver come out that good Cheers Wal
F flyfisherman Well-known member Joined Dec 5, 2011 Messages 89 Aug 4, 2018 #5 Nice looking metal :!: what size are those bars? Weight?
Geo Well-known member Joined Mar 1, 2011 Messages 7,070 Location Decatur,Ala. Aug 4, 2018 #6 They averaged 240g each. It was a half pound mold but they kind of held a little more.