Hello All,
We have around 12 tonnes of copper nitrate solution kept with us. We are looking to recover copper from it. The assay report shows 62 percent of copper in this waste solution. What will be the most economical method to cement out copper from this. We have asked local refineries and they are quoting a very low price (50 cents per kg). With the copper prices skyrocketing we are thinking that it would be better to recover the copper in house even if it takes us time we are ok with it since labour is pretty cheap where I live. We have recovered copper on a small scale before with iron but are unsure what will be the most reliable method to do this on a big scale. Would really appreciate all the help that you give.
I hope you all are keeping yourselves and your families safe during these tough times.
Regards
Gaurav
We have around 12 tonnes of copper nitrate solution kept with us. We are looking to recover copper from it. The assay report shows 62 percent of copper in this waste solution. What will be the most economical method to cement out copper from this. We have asked local refineries and they are quoting a very low price (50 cents per kg). With the copper prices skyrocketing we are thinking that it would be better to recover the copper in house even if it takes us time we are ok with it since labour is pretty cheap where I live. We have recovered copper on a small scale before with iron but are unsure what will be the most reliable method to do this on a big scale. Would really appreciate all the help that you give.
I hope you all are keeping yourselves and your families safe during these tough times.
Regards
Gaurav