Hi as a way to keep regulated and localized issues in one place I'll start this post this way as per 4metals suggestion.
So far I have been able to get most chemicals needed.
As per Lanfears help and suggestion one can get 90 percent sulfuric acid as draincleaner, at a premium cost appr 300 NoK/l OBS bygg
Or one can buy battery acid which should be around 35 ish percent (Very good as it don't contain additives, but may need concentrating)
HCl can be bought at OBS/Jernia and so on in 30 percent for about 100 NoK/l.
It is also available in 36 percent 5 liter cans at wholesale chemical shops(allowed for privates to buy as it has a child-safe cap appr 50 NoK/l )
Hydrogen Peroxide can be bought at farmacies at ludicrous prices. I payed 164Nok for 100ml 10 percent (Had to start somewhere :roll: )
At wholesale chemical shops prices are far better, but the one I'm using sells only in 25L quantities.
Most other chemicals are available at the wholesale Chemical shops as a registered company.
For lab grade chemicals one has to go to shops like Fredriksen and so on. But they don't sell to personal one men companies.
If someone has more information regarding local supplies of chemicals in Norway please share with us.
I think it might even be possible to get it shipped from/to Sweden or Denmark?
Do anyone have any information on the legalities regarding this?
So far I have been able to get most chemicals needed.
As per Lanfears help and suggestion one can get 90 percent sulfuric acid as draincleaner, at a premium cost appr 300 NoK/l OBS bygg
Or one can buy battery acid which should be around 35 ish percent (Very good as it don't contain additives, but may need concentrating)
HCl can be bought at OBS/Jernia and so on in 30 percent for about 100 NoK/l.
It is also available in 36 percent 5 liter cans at wholesale chemical shops(allowed for privates to buy as it has a child-safe cap appr 50 NoK/l )
Hydrogen Peroxide can be bought at farmacies at ludicrous prices. I payed 164Nok for 100ml 10 percent (Had to start somewhere :roll: )
At wholesale chemical shops prices are far better, but the one I'm using sells only in 25L quantities.
Most other chemicals are available at the wholesale Chemical shops as a registered company.
For lab grade chemicals one has to go to shops like Fredriksen and so on. But they don't sell to personal one men companies.
If someone has more information regarding local supplies of chemicals in Norway please share with us.
I think it might even be possible to get it shipped from/to Sweden or Denmark?
Do anyone have any information on the legalities regarding this?