Hi everyone!
So being new to gold refining I thought I would try the citric acid way of removing foils off of some ram sticks. I used 300ml of distilled water and mixed in 25g of citric acid, 20g of salt and 25ml of 3% hydrogen peroxide. Once it was all mixed I added a few ram sticks and set it aside.
After about 5 hrs it looks like the some of the gold fingers have turned a copper colour? is this normal. I would have thought that the foils would slowly drop off since they wouldn't dissolve in the mixture? Is the copper cementing itself back onto the gold?
The liquid is also a bit cloudy but doesn't have a blue or green tinge from the copper either?
cheers
Torx
So being new to gold refining I thought I would try the citric acid way of removing foils off of some ram sticks. I used 300ml of distilled water and mixed in 25g of citric acid, 20g of salt and 25ml of 3% hydrogen peroxide. Once it was all mixed I added a few ram sticks and set it aside.
After about 5 hrs it looks like the some of the gold fingers have turned a copper colour? is this normal. I would have thought that the foils would slowly drop off since they wouldn't dissolve in the mixture? Is the copper cementing itself back onto the gold?
The liquid is also a bit cloudy but doesn't have a blue or green tinge from the copper either?
cheers
Torx