I think your original feedstock can be much more than simply copper over plated with Silver. The addition of unknown metals is what I think is gumming up the process. You are not making copper sulfate by dissolving electroplated copper in sulfuric acid. This would be the preferred method. There is a video in our video section by NurdRage on distilling the nitric and recovering the copper metal. Is this the process you used or was your process a shortcut of some sort?
Yes NurdRage is the process I was trying to work with. And in the process was trying to free up some of the silver to be used for a silver cell at a later time. My thoughts actually was working as expected most of the plating had come off the base metal and was cemented out. A small sample in test tube added some salt water showed a small amount of silver was still in solution. When I weighed up what was left after the first round I figured with the amount of silver that was cemented out I was going to be short on the amount of copper sulfate needed to setup the copper cell so I added the rest of my nitric acid and a couple of the what I thought was COPPER( bronze) bars back in at that time my solution was a bright vivid blue as I was expecting when I got up the next day and checked is when I found the wrong color solution. And the slight mess. But I think I have gotten lucky and am good on the copper sulfate portion just have the silver and tin mess to deal with at a later time. Will dry, roast and store labeled as such. And after rereading hokes book on the part about tin and how to deal will decide whether to melt and scrap or try to separate
 
The extra step of electrolytically recovering the copper from the converted copper nitrate solution (after adding sulfuric) will allow you to leave the other base metals in solution and selectively deposit copper to assure your copper cell will have pure copper sulfate with low impurities.
 
The extra step of electrolytically recovering the copper from the converted copper nitrate solution (after adding sulfuric) will allow you to leave the other base metals in solution and selectively deposit copper to assure your copper cell will have pure copper sulfate with low impurities.
Would it be wise after distilling using this batch of copper sulfate for the first test run of the copper cell and run the rest of the bronze bars I have as my feed or is running bronze asking for more trouble.
This is my first time setting up an electrolytic cell I’m starting very small and using this to learn with I fully expect some mistakes.
It’s going to be small using a 5.7l tote and the power supply is 0-30 volts 0-10amps.
 
Update the nitric acid and copper sulfate have been distilled ended up with 864 grams of copper sulfate and sulfuric acid. Unable to relocate where I seen the recipe for the electrolyte on here I started the copper cell using nurdrage’s video of double the water to copper slurry. This worked good for about 15-20 minutes gave a nice copper plating that would scrap off the stainless steel cathode then stopped. After some more searching found the recipe and the 2.5L of solution was way to concentrated so now I have almost 5 gallon of copper sulfate and water. Used 2.5l in my small cell and added 100ml sulfuric intentional error on the short side of the 250ml per recipe as I figured there to be around 200ml of excess sulfuric in the total solution. Started the cell and 12 hour later it was still going good except when I pulled the cathode the copper looked good but would fall off if shaken
Just added the rest of the sulfuric to the batch and scraped the loose copper off will see the results after work tonight.
The cell has about 14 in2 of cathode so I have the current set at 2.5 amps which has the voltage running between .6-.8 volts before the addition of sulfuric acid now or at least when I left it the voltage was .8-.9 volts at the same amps. Photo of the soft spongy copper IMG_3455.jpeg
 
Here is the recipe for the electrolyte from one of 4metals post
Copper as copper sulfate 45 – 50 g/L
Sulfuric acid 170 – 200 g/L
The following additives, used in very small quantities, are to level the deposit and affect the grain of the deposit making it denser.
Bone glue, 1 gram for every 25 pounds of anode processed thru the solution
Thiourea, 1 gram for every 20 pounds of anode processed thru the solution
NaCl, 0.04g/L
 
Finally I finished reading this thread https://goldrefiningforum.com/threads/electrolytic-copper-refining-cell.24397/
which had most of the answers I need for the copper cell. Cleaned off the spongy copper from my cathode and adjusted the amps down from2.5 amps to about 1.8 amps this had the voltage around .38-.5 volts had been running for about 6 hours when I pulled out the cathode to check before heading to work the copper is plating out very nice even and hard was able to scrap the surface and nothing comes loose. Will pull out tonight to get pictures. At this time there is no additives in the electrolyte just water copper sulfate at about 50g/L and sulfuric acid 180g/L
Will be making up some anode plates this weekend from some pure copper motor windings to get my new cell set up decided on a slightly larger one as the current size don’t have room to maximize the 10amp power supply. The new one with 1 cathode and two anode’s about half full should need about 9 amps the plates are 6”X 11” with fluid level at max level gives 8” usable area with room to add in 2 more of each anode’s and cathodes after finding a bigger power supply
 
Ok have a question I have figured out the current makes a big difference on the plated copper. Too high a current density and it plates out spongy and falls off. But also if run too low it plates out extremely hard and smooth. But in playing with the amps I inadvertently ran a thin layer of super smooth copper on the stainless steel cathode and now after about a week of running at 2 amps which is where it started to dull the copper color but was still hard and nothing would rub off.
Decided last night I would decommission this extra small cell as I’m planning to pour some plates for the slightly bigger cell this weekend. And that’s when I discovered I need some advise before I start the next one the copper plating will not come off the stainless cathode.

I’m thinking if I run the amps high and cause the soft sponge to plate first then without scrapping it off if I drop current down and plate the hard copper on top it might make it release from the cathode when it’s time.

This small one is me learning it was running without any of additives and on pure copper anodes from motor windings. I have also made some uhmw covers for the edges on the bigger cell so it wont plate around the sides and bottom.
My cathodes are made from some leftover 1/4” stainless steel sheet at work not sure what grade it is. Will definitely give the surface a good polish before trying again.

Any advice on how to get the copper to not stick so hard to the stainless cathode that it wont come off would be appreciated thanks
 

Attachments

  • IMG_3476.jpeg
    IMG_3476.jpeg
    1.5 MB
  • IMG_3475.jpeg
    IMG_3475.jpeg
    2.2 MB
Use a copper sheet as the cathode. This is how I did it. This way you just melt the whole thing for later use, or to sell. Using stainless, you will need to protect the edges so the copper won't plate there, and only in thin sheets. You can then flex the stainless and peel the copper from it. The stainless also needs to be perfectly clean as well.
 
Use a copper sheet as the cathode. This is how I did it. This way you just melt the whole thing for later use, or to sell. Using stainless, you will need to protect the edges so the copper won't plate there, and only in thin sheets. You can then flex the stainless and peel the copper from it. The stainless also needs to be perfectly clean as well.
Thanks that’s what I was afraid of was trying to use free stock I had access to with the stainless steel but might have to find a source for some copper sheets
 
Depending on the size needed, you could cut open and flatten copper pipe. If you need bigger you can try copper roof flashing, just be sure it isn't plated copper. I got a 30 foot by 16 inch piece a while back from a roofer that was replacing a copper trimmed roof. I haven't priced any new but I would think it would be expensive. Sawing your new made piece into thinner pieces and keep adding to them might work also.
 
Depending on the size needed, you could cut open and flatten copper pipe. If you need bigger you can try copper roof flashing, just be sure it isn't plated copper. I got a 30 foot by 16 inch piece a while back from a roofer that was replacing a copper trimmed roof. I haven't priced any new but I would think it would be expensive. Sawing your new made piece into thinner pieces and keep adding to them might work also.
I have lots of clean copper from motor windings might try and see how thin I can get some to pour into the anode mold I built or 1.5-2 inch pipe would work also for the width I need
 
If you weave small wire into a sheet it becomes solid as it it works. But some kind of sheet is easier to work with.
 
If you weave small wire into a sheet it becomes solid as it it works. But some kind of sheet is easier to work with.
The stainless ended up working just had to hit the copper with the air hammer and it peeled right off. Just couldn’t hold the plate chisel and hammer to get a good enough hit to break it loose. Going to give it a good mirror polish so it will be a little easier next time.
 