Doing a warehouse sweep and getting ready to blow out a bunch of chips. Was wondering the Cu weight on the Intel Xeon for example.
Quickly jacked off the #2 Cu tops on 3 random chips and the results are below.
82% Cu by weight on the AMD.
67% for both Xeon .. and even the lids are different between the 2 Intels.