- Joined
- Aug 12, 2021
- Messages
- 1,259
A couple of things bother me about Jason's techniques. 1. he doesn't show any base line for wether the ore is basic , or acidic. Other then they are concentrates off his shaker table. Usually a quartz concentrate, since Gold is only associated with quartz. Not too bad showing on pyrite cons assay/smelting 2. he never explains, very well, the reason he uses lead, instead of PbO ( Litharge, assay grade ), wether he is producing a mono, bi, etc., silicate flux. Hire a chemist to explain the difference, in layman's terms A couple more minor grievances, but I will not nit pick too much. He's better then anyone else out there, but then again, I haven't seen any other youtube videos touting our industry. Maybe trade secrets keep is out of the main stream? A shout out to Jason, thanks, fun to learn from you. Also a huge shout out thanks to , is it sreetips, or streetips, seen it both ways. Nothing to complain about with your youtube videos, yet.
A very good idea.MBMMLLC has perfect videos about pyrometallurgy on youtube. Watch them out, you will visually learn a lot about cupelling and smelting.
If I were you, I will try to take like 10g of lead and do a "blank" cupellation - to elucidate wheather the feed is causing problems, or you just do not have equipment/temps/oxygen right.