silversaddle1
Well-known member
Like I had said before, I have half a gaylord full of computer cable ends that I have trimmed off cables and internal connectors(all gold pins in them). I'm guessing well over 800 pounds of them. And there's some pretty old stuff in there, IBM buss & Tag cable ends, Old Winchester ends, etc. Well I found a refiner the does cyanide leaching. I'm wondering if this would be a good way to recover the gold from these pins without doing a ton of work on them. They do all the work and keep 30% of the values. What say you?