dissolve gold

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

ssmontecarlo

Well-known member
Supporting Member
Joined
Oct 8, 2022
Messages
61
Location
Tennessee
Since I'm limited to my mobility for at least 1 more day, I was gonna weigh, than dissolve these small buttons. I have done this a couple times in the past, with losing a tenth of a gram at the most.

I honestly believe they could be refined to a higher purity.
 

Attachments

  • 1668084578606213573218355882502.jpg
    1668084578606213573218355882502.jpg
    3.2 MB · Views: 0
Those are some nice buttons !!!
They appear to have only been refined once ?, If so dissolve & drop again, the melt into a button.
How much do they weigh ?
 
The percentage loss on re refining your gold decreases with the amount you process if you process with care, any losses should be in your waste filters and the stockpot which you can recover later.
 
Yes I keep all filters. Actually I have a beaker here that is just filters used to capture recovered gold and filters used while filtering gold in solution. One thing I have learned, do not throw it out until you are for certain there is no more Au present. And be patient.

Maybe a tenth or 2.
 

Attachments

  • 16681627965107453036622848716397.jpg
    16681627965107453036622848716397.jpg
    2.5 MB · Views: 0
Back
Top