DMG suitability?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Long Shot

Well-known member
Joined
Apr 15, 2014
Messages
202
Location
Belleville Ontario
Hello All,

Living here in Canada provides for a hard time getting some of the chemicals we need to refine at a hobby level. Whether it be regulative restriction, reluctance from chemical suppliers to deal with Joe Shmoe or ridiculous charges for shipping and / or duties the feasibility of obtaining some things is unfeasible.

In regards to DMG my question is this - are supplement grade products suitable for the purposes we seek?

Here is a link to what I'm asking about https://www.vitasave.ca/dmg-125-mg.html .

Thank you for looking.

Long Shot
 
Spelling, spelling, spelling... Why we try to drive it home so hard.

https://en.wikipedia.org/wiki/Dimethylglycine
https://en.wikipedia.org/wiki/Dimethylglyoxime

Which one would you put into your body and which one in your beaker?

Göran
 
Hi Göran - thanks for correcting my ignorance on this. The basic level of organic chemistry I was exposed to in college was about 20 years ago and I recall it was a nightmare for most - many did not pass this course. Confusion arises when both are referred to as DMG. Back to the old drawing board.

Obviously to anyone one else looking at my original post, forget I asked :oops:
 
Long Shot,
"forget I asked :oops:"

I am glad you asked, this kind of question helps you, and all of us.

Not only the importance of spelling, This is also an example of why using abbreviations is not always a good idea. Or that texting can be dangerous, not only while driving.

Devil is in those details.
 