And did it change the way you do business?

I get stuff analyzed all the time...I have a friend who has one and he will shoot things for me. With that, I don't rely upon it, nor do I use it nearly as often as I would if I had one.

Given that the prices have come down so much, I'm just curious, is it something you use almost constantly, or is it just something that makes life a little easier once in a while?
 
We have several at work. Great for sorting alloys. I use them to ball park silver content so as to simplify titration

They're very useful for materials if the proper context is followed and samples without overlapping contaminants are analyzed.
 