Here is a short video I produced to demonstrate the technique I use to drop gold using Stump Out purchased from Home Depot (about $6 per pound).
[youtube]http://www.youtube.com/watch?v=HNq3Tp99XOE[/youtube]
I have gottten good results so far using this process.
Please give comments or suggestions if you see anything improper.
If dropping gold using this method will hinder the recovery of other PMs in solution, then I would like to hear about that as well.
Thank You - kadriver