Your voltage is what you want to be able to adjust. The amperage is the amount of energy it is taking to to do the work and that is determined by the surface area of the ( anode/cathode ) material you are running.


Same principal as using a 100 watt light bulb versus a 60 watt light bub on a 110V electrical system in a house. The voltage stays constant at 110V but a 100 watt bulb uses more energy than a 60 watt light bulb because it produces more light.