Hello everyone i hope you are having a good day!!
And I hope this is the right procedure to ask question about gold refining
I started recovering gold in small quantities in small containers and at the end i ended up recovering more platinum, palladium, copper, silver and small quantities of gold
Lately my friends and customers gave me a lot of phones, computer and other electronics, took them apart and removed as much iron and base metals as possible and wanted to speed up the process i started processing big quantities of boards (5kg) of mixed boards but i ended up with a goo and stuck, not knowing what to do next, luckily i recover everything by cementing and got rid of junk and kill the acids and dispose them
First question: is there another way to refine platinum without boiling?
I don't have space at this moment to set up a heater and let it run for three hours
And i would like to listen yo your advice after you read about the process
I came out with:
I take apart the whole phone or device, remove as much iron, aluminum, plastic and other junk
Big pieces of copper i set them aside
Then i break the board down to small pieces, burn it, put it in a 5 gallon bucket, add hydrochloric acid, leave it for three days, empty and refill again and leave for three days, empty container and add new hydrochloric acid and add nitric acid *** needed to resolve most of the metals (platinum wont dissolve in aquaregia at room temperature) so i set it aside, since i ended up with dirty aquaregia i cement it and removed the copper, boiling the remaining precious metals, wash and save for further refining
(Sometimes i pulverize the boards) just to experiment with the boards
I want to know if there is a way to do this process without boiling l, for the moment i cant set up a stove or heater because lack of space
I attached some pictures of the process
I need your advice please, i think i got more than i can chew, i am talking about maybe 50 kg of cleaned, pulverize boards, i think there is more palladium and platinum than gold in there, i attached some pictures of the materials i have cleaned, the bags feel heavy one of them is about 3 kg
I drop the gold with smd
The palladium with zinc
And platinum with ammonium
If you can help me with your advice i really appreciate it, thanks
And I hope this is the right procedure to ask question about gold refining
I started recovering gold in small quantities in small containers and at the end i ended up recovering more platinum, palladium, copper, silver and small quantities of gold
Lately my friends and customers gave me a lot of phones, computer and other electronics, took them apart and removed as much iron and base metals as possible and wanted to speed up the process i started processing big quantities of boards (5kg) of mixed boards but i ended up with a goo and stuck, not knowing what to do next, luckily i recover everything by cementing and got rid of junk and kill the acids and dispose them
First question: is there another way to refine platinum without boiling?
I don't have space at this moment to set up a heater and let it run for three hours
And i would like to listen yo your advice after you read about the process
I came out with:
I take apart the whole phone or device, remove as much iron, aluminum, plastic and other junk
Big pieces of copper i set them aside
Then i break the board down to small pieces, burn it, put it in a 5 gallon bucket, add hydrochloric acid, leave it for three days, empty and refill again and leave for three days, empty container and add new hydrochloric acid and add nitric acid *** needed to resolve most of the metals (platinum wont dissolve in aquaregia at room temperature) so i set it aside, since i ended up with dirty aquaregia i cement it and removed the copper, boiling the remaining precious metals, wash and save for further refining
(Sometimes i pulverize the boards) just to experiment with the boards
I want to know if there is a way to do this process without boiling l, for the moment i cant set up a stove or heater because lack of space
I attached some pictures of the process
I need your advice please, i think i got more than i can chew, i am talking about maybe 50 kg of cleaned, pulverize boards, i think there is more palladium and platinum than gold in there, i attached some pictures of the materials i have cleaned, the bags feel heavy one of them is about 3 kg
I drop the gold with smd
The palladium with zinc
And platinum with ammonium
If you can help me with your advice i really appreciate it, thanks