joem said:
alexxx said:
In Quebec you can sell your weee plastic between 0.06 and 0.15 a pound depending on color, type of polymer and if it is clean of contaminants such as metals, dirt, etc...
To who? oh and Alexxx I had a pick up for you from my niece in Laval, but her boss paid someone $300 to removed e-waste.
Feel free to hit me up anytime if you have any pick up leads, I will give you 25% of my profit.
1 514 965 five five five five
Ge ep or Si ms probably took the load... :evil:
For the plastic, I usually buy clean ABS at the following prices (no steel, no screws, no trash of any kind) :
white : 0.08 / lb
black : 0.07 / lb
mix colored : 0.06 / lb
needs to be balled or into gaylord boxes (gaylords are not really good since shipping will kill you)
You can check with EDI, I believe they will buy it at a fair price (they are very nice people to deal with).
FC M, E-c ycle , Ge ep and Si ms will buy it too, but it's always better not to feed to big boys in my opinion. They have enough of the pie + their prices are not the best ones around. I always prefer to sell at a lower price instead of selling to them...
Or you can check for a local ABS pipes manufacturer, they will be able to pay you up to 200 a ton if 100% clean (many of them also take it in a shredded form). If shredded you will fit way more material into a box to save on shipping and its easier to remove ferrous components with a magnet.
cheers,
Alex