Machine shop owner told me he did some work for a guy that was stripping tons of tin plated electrical contacts. Was looking at bins full of copper, the owner told him the money was in the tin. I'd like to recover Sn also, but this forum doesn't seem to be the place to ask those questions.
I think Tin is a magnitude harder to sell at prizes comparable to the Spot than Gold.
But if you are in contact with the ones that can buy at good prizes it is always interesting.
Even better if one can share those details.
Agreed it is slightly outside our scope, but we want to reclaim both metals and values so why not.
 
Machine shop owner told me he did some work for a guy that was stripping tons of tin plated electrical contacts. Was looking at bins full of copper, the owner told him the money was in the tin. I'd like to recover Sn also, but this forum doesn't seem to be the place to ask those questions.
I am very interested in seeing the before and after pictures of these Electrical contacts, I think this "Tin " is infact Silver Solder.
 
I am very interested in seeing the before and after pictures of these Electrical contacts, I think this "Tin " is infact Silver Solder.
I wasn't involved first person.
Copper9,796.240.11USD per Ton10/4/24 10:23 AM
Nickel17,598.50-1.77USD per Ton10/4/24 08:06 AM
Zinc3,143.500.30USD per Ton10/4/24 10:08 AM
Tin33,801.50-0.01USD per Ton10/4/24 08:44 AM
At 3.45% X the price of Cu it is feasible.
 