semi-lucid
Well-known member
Hello all.
I've been reading some comments about Electrowinning scattered in various threads, and I thought I would start a dedicated thread.
There was some discussion in last part of this thread:
http://goldrefiningforum.com/phpBB3/viewtopic.php?t=1093&postdays=0&postorder=asc&start=30
And then "goldsilverpro" stated;
"I've plated out nickel or copper onto 300 series stainless sheet many times, with great success."
http://goldrefiningforum.com/phpBB3/viewtopic.php?t=1092
Could your tell us the details of your Electrowinning process?
Is there any possibility this is a practical way to process bare printed circuit boards?
Regards.
Semi
I've been reading some comments about Electrowinning scattered in various threads, and I thought I would start a dedicated thread.
There was some discussion in last part of this thread:
http://goldrefiningforum.com/phpBB3/viewtopic.php?t=1093&postdays=0&postorder=asc&start=30
And then "goldsilverpro" stated;
"I've plated out nickel or copper onto 300 series stainless sheet many times, with great success."
http://goldrefiningforum.com/phpBB3/viewtopic.php?t=1092
Could your tell us the details of your Electrowinning process?
Is there any possibility this is a practical way to process bare printed circuit boards?
Regards.
Semi