I love Christmas- I can take 2 weeks off and spend some quality time emptying my sacks and making some good gold without the phone ringing!
Here's a couple of them ready to empty and get processed. The right hand one is 31Kg (68.31 pounds) of close cut fingers- mostly telecoms. The left is 27Kg (59.53 pounds) of ceramic processors mostly telecoms.
I usually post up some form of competition at Christmas time so not being one to break with tradition let's have another.
Just for giggles of course! How much gold do you think I'll get?
Here's a couple of them ready to empty and get processed. The right hand one is 31Kg (68.31 pounds) of close cut fingers- mostly telecoms. The left is 27Kg (59.53 pounds) of ceramic processors mostly telecoms.
I usually post up some form of competition at Christmas time so not being one to break with tradition let's have another.
Just for giggles of course! How much gold do you think I'll get?