engelman said:I sent this metallic piece to friend who work in professional lab and he put it in nitric to separated all the metals and to get only the gold.
He sent me the picture with black powder (which he says it is gold). photo attached.
Gold is not the only thing that won't dissolve in nitric acid.What i meant was that the metal piece that I melted was sent to a friend lab.
He use nitric to separate it from the copper and he got this black dust (gold).
What i don't understand is how come the assay didn't find anything while the other did found.
and if he wanted to salt it, he can done it as well with the sample for the assay.
Yeah, you are crazy or it is a scam. 3% is an ounce per kilo, or 1300 dollar per kilo of dirt. Your small sample with the black powder looks like less than 1/10 of a gram, making your original sample at most 3-4 grams.engelman said:I will say something more. and you all will think i am crazy or its a fraud etc.. the owner says that he got no less than 3% of gold por metric ton. means 30kg of gold for each ton. he say that there is way more but he can guarantee it, as well Rhodium, Platinum, Palladium.. and again, no money needs to be sent upfront, he say to me- ¨bring your people you trust, we will send them few tons of soil, they will separated the gold and they will pay me after¨ all he want is to be present when they extract it.
I don't have a refinery yet, there are plans for the future but I have been short in cash and time. I do all my refining outdoors so I can only refine during summer, but spring is here and I have just started up doing experiments so I can test your sand too.engelman said:didnt thought you will say different.
Do you have a refinery ? do you know how to extract the gold? if so i can offer you 2 things.
1. come with me to there and we will see all.
2. I will send you 500g of sand. you will tell me your results.
Another question. did you saw the photo with the mercury? what is your opinion about it?
Your "friend", the land owner, is adding powdered gold dust to the carefully selected spot that he shows you he is "sampling". Therefore you get the 3% figure from that carefully selected "sample". When you take a larger sample, an send it to a lab, of course there is no gold.engelman said:I am confused, can any body help me to get idea of what is going on here?
Thank you.