yes. incinerate the varnish, or strip it with solvent, then desolder legs, put them into crucible, add measured ammount of silica and bake it slowly to temperature.
Silica? What role does it play in the process?yes. incinerate the varnish, or strip it with solvent, then desolder legs, put them into crucible, add measured ammount of silica and bake it slowly to temperature.
Read that postSilica? What role does it play in the process?