Ferrous Sulfate - Did I buy the wrong thing?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Yesterday I put copper tubing in the liquor... this mornind something was precipitated... i'll leave the copper inside the solution untill monday and i hope to find something more
 
Assol said:
Thanks all!
the board are new but descarged from production. The producer told me that he use not less than 0,6 g/kg... are big 40cm x 20 cm.... as soon as i've got picture i'll send it.
Grazie

G is right, the little bit of gold got precipitated in your second picture above, where the 500g of smb was added.

I know the producer told you that he used no less than .6g/kg......but, this is the precious metal game, and to take a seller at their word, is the fastest way to get played
 
Hi,
Before the dissolution in AR, i had 98 gram of solid in the filter.
Afrer dissolution in AR , I had only 41 grams of solid stuff.
This is the picture of solid stuff... just same plastic, i think.
grazie
 

Attachments

  • IMG_3887.JPG
    IMG_3887.JPG
    1.5 MB · Views: 85
  • IMG_3888.JPG
    IMG_3888.JPG
    2.9 MB · Views: 85
Back