Good evening everyone,

Long short of the story is I have a few fiberglass CPUs, I took them outside and held a butane torch to them to melt the solder to that I could remove the pins. After getting all the pins out I got the idea to take an exact o knife to the now charred pin-less remains. As I peeled the layers back one at a time about the 3rd one down contained a bunch of connections that have the look of copper. The further down I go the more layers are littered with these connections. I'm wondering if anyone knows what metal they are & if they are inside ceramic cpus as well?

R/S

Sgt Heisler
 
Check out this post:

Fiber CPU Dissection

and

Fiber CPU Epoxy Center]

Most of the layers are simply copper connections, but there are a few key areas with gold plating as seen in the links above.

Incinerating components can produce very deadly gases. If you are incinerating, be sure to use proper fume control.

Steve
 