Hello once again, I am hoping to get help in understanding the results from two ore/ rock samples that I recently had done?
Two Samples supplied. Both 31.0 grams each
Sample Preparation -
Pulverize up to 250 g 85% <75 um
Analytical Procedures
Au-AA23. Au 30g FA-AA finish
Instrument. AAS
Sample Description
Method. Au-AA23
Analyze. Au
Units. ppm
LOD. 0.005
~~~~
TAZ-20. 0.313
Target Range- Lower B. 0.279
Upper B. 0.325
Blank
Target Range- Lower B. <0.005
Upper B. 0.010
ORIGINAL 0.259
DUPLICATE. 0.220
Target Range- Lower B. 0.223
Upper B. 0.256
———————
ORIGINAL. 0.122
DUPLICATE. 0.133
Target Range - Lower B. 0.116
Upper B. 0.139
——————-
Sample Description
Method. WEI-21. Au-AA-23
Analyze Recess. Wt. Au
Units. kg. ppm
LOD. 0.02. 0.005
Sample #1. 0.03. 1.170
Sample #2. 0.03. 2.38
===============
Well that’s what I got so hopefully someone can help interpret this for an old timer?
Thanks All
Two Samples supplied. Both 31.0 grams each
Sample Preparation -
Pulverize up to 250 g 85% <75 um
Analytical Procedures
Au-AA23. Au 30g FA-AA finish
Instrument. AAS
Sample Description
Method. Au-AA23
Analyze. Au
Units. ppm
LOD. 0.005
~~~~
TAZ-20. 0.313
Target Range- Lower B. 0.279
Upper B. 0.325
Blank
Target Range- Lower B. <0.005
Upper B. 0.010
ORIGINAL 0.259
DUPLICATE. 0.220
Target Range- Lower B. 0.223
Upper B. 0.256
———————
ORIGINAL. 0.122
DUPLICATE. 0.133
Target Range - Lower B. 0.116
Upper B. 0.139
——————-
Sample Description
Method. WEI-21. Au-AA-23
Analyze Recess. Wt. Au
Units. kg. ppm
LOD. 0.02. 0.005
Sample #1. 0.03. 1.170
Sample #2. 0.03. 2.38
===============
Well that’s what I got so hopefully someone can help interpret this for an old timer?
Thanks All