Hi all,

my first try with silver :)

1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...

14. I think,this yellos powder is gold and palladium,

15. tomorrow ' s continues


mocodos
 

Attachments

  • 6.jpg
    6.jpg
    210.4 KB · Views: 433
  • 5.jpg
    5.jpg
    23 KB · Views: 433
  • 4.jpg
    4.jpg
    175.9 KB · Views: 433
  • 3.jpg
    3.jpg
    217.9 KB · Views: 433
  • 2.jpg
    2.jpg
    108.1 KB · Views: 433
The yellow powder is not Au or Pt. I would guess it's a tungsten compound (oxide ?) or some other metal compound.

Steve
 
mocodos said:
Hi all,

my first try with silver :)

1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...

14. I think,this yellos powder is gold and palladium,

15. tomorrow ' s continues


mocodos

Dear Mocodos

I am also looking for the same to make silver powder.

Pls kindly help me.in detail to amke silver powder.What raw amterail and cell you use.
regards,
robin
 
mocodos said:
Hi all,

my first try with silver :)

1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...

14. I think,this yellos powder is gold and palladium,

15. tomorrow ' s continues


mocodos
Howdid you made it?

what is white metal sheet made of?
Waht is the black rod is ?
2 OZ circuit breaker contacts?
. cementing with copper? what does it mean I am new to this term.
some heating the AR?
What is the powder size>

Pls kindly send me the detail for the same.
 
mocodos said:
Hi all,

my first try with silver :)

1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...

14. I think,this yellos powder is gold and palladium,

15. tomorrow ' s continues


mocodos
Please kindly show me your more cell picture so I understand bettter.
rgdds
robin
 
please35 said:
Howdid you made it?

what is white metal sheet made of?
Waht is the black rod is ?
2 OZ circuit breaker contacts?
. cementing with copper? what does it mean I am new to this term.
some heating the AR?
What is the powder size>

Pls kindly send me the detail for the same.

Use the SEARCH function, look up Hokes book. Get some reading done :)
 
dcurzon said:
please35 said:
Use the SEARCH function, look up Hokes book. Get some reading done :)

I second that. This forum contains everything you need to know, plus alot more. You won't get much help if you expect people to hold your hand. I highly recomend lazersteves DVDs if you need visual help getting started. Read the silver threads, hokes book, and you'll be well on your way.

Good luck~!
 
copper_corn said:
dcurzon said:
please35 said:
Use the SEARCH function, look up Hokes book. Get some reading done :)

I second that. This forum contains everything you need to know, plus alot more. You won't get much help if you expect people to hold your hand. I highly recomend lazersteves DVDs if you need visual help getting started. Read the silver threads, hokes book, and you'll be well on your way.

Good luck~!

thanks
it doesnot mean I didnot read.but there are so many file so I asked for your help.to locate the thread.
rgds
robin
 

Latest posts

Back
Top