my first try with silver
1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...
14. I think,this yellos powder is gold and palladium,
15. tomorrow ' s continues
mocodos
my first try with silver
1. 2 OZ circuit breaker contacts
2. decompose with nitric
3. cementing with copper
4. washing 6 times with water
5. decompose with nitric acid (without heat) to made a solution for silver cell
6. !!! i have found some yellow powder !!!
7. filter the yellow powder
8. silvernitrate to silver cell
9. yellow powder to AR to test the slime/yellow powder
10. some heating the AR
11. "after heating the yellow powder will not dissolve at all"
12. test with stannous...
13. test silver cell...
14. I think,this yellos powder is gold and palladium,
15. tomorrow ' s continues
mocodos