Floaters in AR? (Algae!)

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Brett Novak

Well-known member
Supporting Member
Joined
Jun 22, 2023
Messages
115
The best way to describe it is floating algae. These are 2nd run CERDIPS in AR after a 20 day AP soak. I've run this before but this is the 1st time with the floaters. Any ideas what they are? Maybe it's the excess peroxide forming a layer?

I'll capture and re-refine it anyway but just wondering if anyone else has seen this.

BN
20230821_182004.jpg
 
Guessing iron compound.

I've never used AP for cpus.

Gather the yellow powder and perform standard metal salt identification testing.